Different heavy sand placers are mainly composed with Iimenite, Zircon, Rutile Monazite and Xenotime. On all X-rays diffraction patterns, I still have high intensity “d-spacing” 2,34 - 1,65 - 1,48. which don't correspond to the here above minerals. Anyone can help or advise ? Has an XRD ever been good for you to do Mineral determination?