Mill Steel Charge Volume Calculation

We can calculate the steel charge volume of a ball or rod mill and express it as the % of the volume within the liners that is filled with grinding media. While the mill is stopped, the charge volume can be gotten by measuring the diameter inside the liners and the distance from the top of the charge to the top of the mill. The % loading or change volume can then be read off the graph below or approximated from the equation and calculation:

% Steel Charge Loading in Mill = 113 – 126 H/ D

 

ball - rod mill charge calculation - estimation
Ball Mill Charge Volume Calculation
  1. Charge Volume of a Grinding Mill (Method 1)
  2. Charge Volume of a Grinding Mill (Method 2)

Nordberg Process Machinery Reference Manual