How Abrasion Index affects Wear Rates

What is the relationship between Abrasion Index affects Wear Rates of steel ball mill and rod mill liners as well as the wear life or consumption of grinding balls or rods.  A little bit of data on crusher (gyratory and roll) liner wear life in also shown.

How Abrasion Index affects Wear Rates

Rubber wear data.

abrasion_index_testing
https://redesign.911metallurgist.com/equipment/abrasion-index-tester/