Hi
I am working in a quartz processing plant.
We have a VSI and after the sieve the output is with 1-10mm -50% and <1mm -50 %.We can separate the iron particles from our permanent magnetic bars(15000 Gauss) for the range of 1-10mm. But we couldn't for the ones with <1mm.