We are making roadbase on a new basalt site, we are struggling to make fines with our jaw screen cone circuit . To get the gradings within the envelope we have to import up to 30% fines, my question is what would be better - to introduce an impactor? a VSI? Or a cone with a sand head ? Or turn our cone into a sand head and introduce an impactor ? Thanks in advance