Do you think it is possible to get an overflow of 1% solid by weight with the right water balance requirement in high rate thickeners or in a gold processing plant? I believe not. Why I am asking you this is, because the plant I got engaged got an overflow of 1% solid by weight almost everyday. What I thought is, if they had been using the correct water balance calculation, it difficult to get a 1% sbw. It is so diluted. Is that possible?