Hi
Does anyone have recommendations on the dissolved oxygen for the SO2/air process.
I could reach to 5-7 g/g SO2 to CN ratio and 8-10 pH ranges with 50 ppm of Cu but almost no recommendation is there in the literature regarding DO.