- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Thickening, Filtering or Tailings and Water.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
Hello there, am interning at a gold mine where there are problems with the clarity of the overflow of the pre-leach thickeners. Initially, only flocc was used at 0.1% strength. Now we are testing a coagulant as well at different dilutions on the plant. The clarity has improved over the 2 weeks we have been testing. How do I make sure the coagulant and flocc compliment each other in the overall clarity and settling performance?