Portable propane-fired Metal Melting Kiln designed to melt precious metals with speed and ease. Melt 1 to 5 oz of fine placer gold (1 to 3 oz silver).
The Melting Furnace Kiln has a straight/vertical chamber and is a bit taller. The mini graphite crucibles are custom-made for the kiln. Other sizes will not fit properly.
The Kiln is designed to be heated with 2 pencil tip PROPANE torches simultaneously. Mag-Torch MT-200 pencil tip torches are highly recommended by our designer, for being more stable. They are an ‘all position’ torch and work well with the propane bottle on its side, are all brass, and are made in the USA.
Please note: We cannot warranty any Kiln heated too high, improperly, or in a manner that goes against their design. This includes using other types of torches or using Mapp gas, which gives off more heat. We recommend using propane only.