Hi.
We have a bank of 6 DR24 Sub-A cells which we are recommissioning. These are self-aerating though want the ability to add LP air to increase the pull rate if need be. Would anyone know where this air should be added? According to the original manual it is from the bottom of the cell though i cannot see any inlet. What we have may be a newer, or older version than the manual. Could it be the 1.5" threaded inlet on the float mechanism as pictured?
Thank you
Brant