I am trying to upgrade bismuthinite to 10% from bulk float conc. containing pyrrohite, pyrite & some copper minerals. Currently using lime and NaCN to depress gangue minerals. Has anyone done this before? Am not yet looking at slurry electrowinning process bismuthinite, no.