I work in the gold mine mill were we extract gold and silver from both oxide, sulphate and transitional ore at mill rate of 680 t/h, just now we introduce NaSH replacing copper at flotation other reagent in place froth, promoter, PAX.
What will be the best recommended dosing rate for the NaSH for such density at 27 to 29%