Hello guys,
I have a question about gold flotation. In a gold flotation plant, grade of feed, before ball mill, is 0.5 ppm but grade in cyclone overflow is about 1.2 ppm. I appreciated if you help me about the mentioned grade difference.
Also grade of ball mill discharge is higher than input feed.