I have access to a Copper-Molybdenum tailings site with the following mineral content present (grams/ton): Bismuth - Bi (0.9), Selenium - Se (0.7), Tellurium - Te (0.4), Rhenium - Re (0.15), Gold - Au (0.015), and Silver - Ag (0.5). I am having difficulty determining it any of this is commercially exploitable, individually or in combination. I would appreciate and advice and opinions. Thank you.