Hi All,
I just received our sample tests back by SGS and I need some help in understanding the fire assay weights measured in Grams/Ton and backing that into what we are measuring in our placer op of Grams/Cubic Meter.
Can I just divide the Ton number by 1.6, the factor I use to convert my M3 volume into tons?
Thanks for your help,
Ghana Bob