I ran 6.11% copper oxide on a shaking table optimised to process chromite ore, and got 10.60% in heading, and 4.28 in middling. Copper was milled at 100 plus mesh. There was no control and hence no optimisation.
How much say 1% copper ore can be upgraded to?