- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Gravity Separation/Concentration.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
We always come across some customers who want to concentrate the alluvial gold .
And their alluvial gold is with some magnetic mineral,so some magnetic would stay with after gold centrifugal or jig separator . below is the flow offer by some suppliers.Could you give us some suggestion about the flow :
My doubt: is the jig separator necessary in the flow ? is it better ,if we put the magnetic separator after trommel prior to centrifugal ? can we separate the magnetic material without magnetic separator ,because we don't need magnetic as concentrate .