We installed our iCon i150 some time back but something isn’t ok as there is no separation of gold and black sands despite following all the procedures. I wonder if there is perhaps a problem with
the electric engine RPM not being high enough....Any thoughts....
Half the black sand falls thru the proper outlet, the other half goes where there should be only gold......