- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Gravity Separation/Concentration.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
Dear All
I want to remove mica fram a +63-315µm sand.
If possible I would like to do it without flottation, is it possible to do it with hydroclassifier (counter-current washer like floatex, hydrosizer or lavodune) ?
Or with spiral classifier ?
Something else ?
I know that this can be done by flotation. What kind of reagent should I use ?
Kind regards