Using gravity concentrators like spirals or jigs, how is the water distribution estimated or calculated between Concentrate and Reject/tailings?
During preparation of the Flow sheet from lab results we came across water balance of the gravity concentrator . It is difficult to assume how water is redistributed/split in between concentrate and reject part of the feed. Water distribution actually depends on Particle Size Distribution PSD and quality of the concentrate and reject.