Dear All,
I would appreciate your opinion, if you could give me some indication on our ball consumption at our factory, do you think that there is a room for significant improvement?
I am attaching the basic data sheet of our zinc-lead mine/factory.
Bond work index
Abrasion index
Specific ore weight
Size of incoming ore in Mill in mm
Product
%
(µ)
Mill diameter in meters
Ball consumption/processed ore - kg/tonne
Electricity consumption per processed 1 ton of ore
in kW/h
11.4
.26-.28
3,1 t/m³
35mm
63% -74 µ
2.7 m
600 gramm/tonne
22 kW/h
Regards,
Boris