Hi everybody,
During performing some Ultrasonic Testing (UT) to measure the thickness of the mill discharge trunnion I found excessive wear. I can say it is in a critical state.
Everything indicates that slurry seeped underneath trunnion or shell liners and start washing the internal part of the trunnion. Probably the mill has operated for long periods of time causing excessive wear to the trunnion with the problem undetected.
Wondering if somebody could help me and give some orientations.
Please have a look at the attached document.
Regards,