For an existing concentrator (with existing installed crushers and mills) where a new deposit is being locked at. What comminution tests should you do?
I would have thought SMC and BBMWI are a must, with maybe UCS and crushing impact tests also important.
I would have though abrasion tests are much less important. Particularly if there is going to be no new equipment capital invested.