The smaller cylpebs have all migrated towards the feed side of the mill, and the larger cylpebs are at the discharge end. What do you think causes that? Does anyone have advice other than dropping the charge, to bring the media back to large on feed side and small on discharge side?
Also, would this affect the recirculating load in the mill circuit?