Looking at dry grinding material of extreme hardness holding a BWi of 27kWh/t from an F80 of 6-8mm to a P80 of 16um in an air-swept compartmented ball mill. There are operating plants doing this to 75um, is 16um too fine? Only considering milling technologies due to project requirements. Any experiences would be appreciated.