- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Grinding.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
Running this dirt in any gravity separation I've tried induces packing/plugging and gold loss. All kinds of sluice setups & centrifuge. Centrifuge struggles and is too little production. Looking at Hydrocyclone for results? Problem areas are mainly 30- to 40+ mesh. Also have high % quartz at times.