Hi my friends
We production dry Iron Cocentrate with grade 65.5% without water. One of our problems is to grinding iron ore up to 75 microns.After charging balls in the mill, larger(50&40mm) balls at the end of the mill and smaller balls(25&30mm) mills are located at the beginning of the mill,which reduces the effective grinding.Is it possible to dry the ball mill with a 75 micron product? Is there a way to avoid moving bigger balls in the mill?
characteristics ball mill:
Mill length=6m
Mill Diameter=2.2m
F80=2.5mm
P80=156micron
Types of balls=50mm,40mm,30mm,25mm