Hi, there. Currently our open-circuit, wet overflow rod mill 6ft x 12ft, feed size <50mm, product size 90% < 2mm has a 14mt/hr throughtput. We would like to triple throughput capcity to 42Mt/hr per rod mill. What would be the scale up dimension of the new rod mill which has 42Mt/hr throughput capacity, given feed and product sizes remain unchanged?