How can we calculate the power of a SAG mill in a SAB circuit for a greenfield project. From Morrell's Power based equation, we can calculate the total energy for the circuit, but how can we split the energy between SAG and ball mill from the total energy? What would be an appropriate transfer size for SAG power calculation for a new SAB circuit? or if there are other equations available for this (not involving transfer size).