Arsenic content in non refractory gold ore (1 reply and 1 comment)

m
ecublens
2 years ago
ecublens 2 years ago

Hello, there is some arsenic in an oxidized gold ore analysis. It is not in the form of arsenopyrite. I thought it was acting with antimony, but the Sb content is also very low. Could you give an idea what the arsenic here might be acting with?

J
Jorge
2 years ago
Jorge 2 years ago

Other possible arsenic minerals could be Orpiment (As2S3) and Realgar (As4S4). If the ore contents silver, proustite (Ag3AsS3)

C
Eng. Cosmas Wambura
1 year ago

Can these arsenic minerals affect the recovery of gold?