Elution (1 reply)

A
EAKUVI
1 year ago
EAKUVI 1 year ago

What causes high Barren eluate

Mike
1 year ago
Mike 1 year ago

Many things.

Process design, process operational upsets, improper chemical addition, wrong chemicals, poor maintenance, bad lab work, water quality changes, bird droppings, people using the process as a bathroom (yes it does happen and can really upset performance), to name a few.