How best can I process gold in kaolin or china clay (1 reply and 1 comment)

R
Rutendo Praise
2 years ago
Rutendo Praise 2 years ago

I have a few tons of china clay, and a sample showed good results, but then the clay is fine and may give me problems processing it. Is heap leaching the best way to have the highest recovery?

J
Jorge
2 years ago
Jorge 2 years ago
1 like by David

You can consider an agglomeration process ahead of the heap leaching process. Follow the link below to read some technical information. It is necessary to perform a testing program to determine the operating parameters (e.g. particle size, cement, NaCN consumption)

https://redesign.911metallurgist.com/agglomeration-heap-leaching/

 

R
Rutendo Praise
2 years ago

Thank you