hello everyone i am an operator in gold plant and i would like to ask some question and i hope i will find the answers for it:
our CIL tanks are 3000 m3
1- what is exactly the O2 does in CIL circuit
2- why is the total cyanide available high at CIL tank nu 8 around 160 ppm
and in tank nu 2 around 270 ppm ?