HI,
we are currently working with the project of processing fly ash (source Venezuela) and producing vanadium pentoxide from the same. We are fusing fly ash with sodium salt and then leaching the resultant to produce AMV and then vanadium pentoxide. but as the fly ash also contain Nickel which we want to remove from product. what could be the way-out for the removing nickel.?
if there is any other method please advise that also?
waiting for help!!!