Good day to all!
Please provide hand.
 
What is the most secure way to separate iridium from osmium metal?
Mike
2 years ago
Mike 2 years ago

While there are more exotic methods using selective leaching and recovery using ion exchange technology the old way is simplest.  https://www.scientificamerican.com/article/separating-osmiam-iridiam-from-gold/

 

A
Metallurgystudent
2 years ago

Thanks a lot for your help.