hello i have been trying to vat leach a sulfidic gold ore using cyanide at 0.2% and a pH of 10.5-11 but gold of about 3g/t is still reporting in tails after 40 hours of leaching from a head of 5.88 g/t. HELP...vat leaching is the only method i can use because of limited resources. thank you