how can the ore described below be pre treated in order to achieve high gold recovery using VAT leaching plant?

arsenic 9382ppm,sulfur 42679.67ppm and gold 6.26ppm

Mike
4 years ago
Mike 4 years ago

Step 1: Run some leach tests.

Step 2: Scale up the testing.

T
Todd H
4 years ago
Todd H 4 years ago

Step 1 is always lab testing!!!!  This ore may or may not need pretreatment but leach tests will tell you.  Pressure oxidation, biological oxidation etc will follow once you know the baseline leach results.

 

Regards

Todd Harvey - Global Resource Engineering http://www.global-resource-eng.com

Miya
4 years ago
Miya 4 years ago

find some lab to run the leaching test