- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Mineral Processing or Laboratory Work.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
How do you determine screen cloth sizes for limestone crushing. An existing lime crushing plant produces 0.5 mm to 1.5 mm finished product using a double deck vibrating screen with mesh No. 8 on the top deck and 12 mesh on the second deck. Aren't the screen clothes sizes too big for the target product sizes?