Hi All,
Does anyone have experience with representatively sampling dry/moist concentrate?
After filtering, the concentrate is transported via conveyor belt (As usual).
There are several places to install a cross belt sampler, however, I have never worked with these samplers nor seen then employed in other operations for this duty. It seems that the conveyor profile must match the cutter trajectory which feels a little fiddly and hard to design correctly.
There are also places to install a cross stream sampler but I am not sure if this will function well with a concentrate which can be moist and clumpy. It seems likely that the sampler would be particularly prone to blockages.
Is it a fools errand to try and take a representative sample of dry (10% Moist!) concentrate?