Anyone has experience for reducing/removing As and Ni from U Uranium Ore Slurry?Our As and Ni is almost 120-150 times more than McArthur ore. The mining method is different too. They have facility for blending the ore as they have dry ore while our mining method is JBS which gives us whatever is in the ore cavity in slurry form directly to ROMs. There is no blending or dilution facility in Cigar Lake.