How many do I have to sampling for analysis assaying of metal in crushed PCB(Printed Circuit Board)? I sieved that 6-7 fraction.I'm very eager for successful sampling. Actually I got different results whenever I analyze PCB and Electronic components. That's big problem to estimate those value.
'6-7 fraction' means sizes(divided into 6-7 size range from 2mm to 125 micron meter)