Hi all,
Our ore/float concentrate contains pyrite and arsenopyrite. I require a high arsenopyrite concentrate with as little pyrite in it as possible for some leaching testwork but have not had any luck. Does anybody have any experience with this? I have tried using several reagents like hydrogen peroxide to float the pyrite out of the bulk concentrate, but the remaining concentrate has a low grade.
I would be happy to buy a laboratory quantity of an external arsenopyrite concentrate but it doesn't appear to be sold by anyone.
Thanks for your help