What could be the cause of getting different Head grades from two plants which receives the same Ore type from the same mine? The feed to the plants is only split by time or silo availability.The two plants uses FAG mills in close circuit with a classification screen. The one plant is consistently showing higher feed grades to the primary rougher float than the other. What affect the grade output from a mill?