hello metallurgists. we have had an issue of importing HCL to our gold processing plant. delivery date is getting delayed. however, we do have stocks of 55% H2O2 in our site. do you think it is possible to replace HCl with 55% H2O2 for carbon washing prior to kiln regeneration furnace.