- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Pyrometallurgy and Electrometallurgy.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
I am running some test using a lab size EMEW cell. I am told to use a certain current density, how do I calculate that? The cathode is 1.5 " diameter by 16" long stainless steel and the anode is 5/8 " diameter by 16 " long titanium.