hi guys. my question is a small scale process. we desorb gold-cyanide (AuCN)) from a carbon. i am currently trying to decompose gold from cyanide in a 1M of NaOH solution. i use stainless steel as a cathode. battery as a power supply. however the problem comes with anode. i cant have nickel in my area. can you guys inform me on other alternative to nickel. and is it necessary to raise the temperature or should i keep it to 25-30 degree centigrade. thanks.