I seem to be losing half of my lead collector metal during my smelt.
My smelt consitentcy usually needs several reapplications of borax after already adding in 2x the sample weight of borax and 1x the sample weight of champman Flux.
Its usually a very thick smelt until I get it to thin out enough and it cools before all of the metal collects at the tip of the cone mold, there's dull Grey particulate all throughout my black glass slag
After the pour cools, my lead collector metal is half of what I started with.
When I place the lead button on a cupell and put it in the muffle furnace, my result was a dull golden crystalline substance mixed with some type of silver colored metal crystalline substance.
I'm a whole slew of issues and I realize that but I'm determined so what and where should I start adjusting?