- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Pyrometallurgy and Electrometallurgy.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
Hi Team,
I getting trouble to improve fineness on Dore' as most of the time i am getting more 50%+ Ag, Is there a specific flux recipe or extra additive that has been tested to improve the fineness of the gold bars?