Hello everyone, could someone tell me a company that sells a complete solution for roasting + gas treatment? It's for gold ore.
My need is to process 200,000t at a rate of 20 to 30 t / h, depending on the roasting capacity. I will use a maximum temperature of 650 ° C.
This ore is dried in a tailings dam.
Mineralogy: quartz, chlorite, muscovite, albite and illite
Fe = 6.1%
C = 4.3%
S = 0.8%
As = 0.3%
Cu = 269ppm