9
REPLIES
3699
VIEWS
Started by
Can you share any news on the proven technology Paste Thickeners and its applications?Not all tailings can be converted to paste with thickeners, depends on the rheology. Only the filter can but at very high cost. The paste formation is still un...
D
Last commented on by diegoottoni
Which mine was this, Victor?
5
REPLIES
1853
VIEWS
Started by Bob Mathias
How to settle Sepiolite clay fines? I need help settling sepiolite clay fines from saline process water. Anyone out there with experience?Am trying to clean Mg4Si6O15(OH) 6H2O in a cemented (Duricrust) layer. It does have a fibrous structure at a s...
Last commented on by David
And http://911Metallurgist.com/C/DIFFERENTIAL%20SETTLING%20TENDENCIES%20OF%20Clay%20Minerals.pdf from www.clay.org
14
REPLIES
3888
VIEWS
Started by
Silica Sand Dewatering: Cyclostack VS Fish Tail CycloneI am looking for experiences in sand dewatering. Any experiences with the cyclo-stack or similar fish tail cyclones? The should be able to dewater to +80% , increasing solids of the underflow.E...
Last replied to by
Actually, in the original Linatex Australia days the set up included a cyclone separator featuring an overflow box which sandwiched the vortex finder plate between it and the tangential entry feed box...
6
REPLIES
8220
VIEWS
Started by Victor Bergman
How much flocculant, with concentration of 0,05 % (m/m), must i add (dosage) in L/min to a thickener with a feed rate of 600 t/h?
Last replied to by Victor Bergman
Thank you all for your input. we managed to diagnose the problem i.e. it appeared that the concentration of our flocculant was insufficient and due to the change in season the temperature also had a n...